Effect of pressurized steam treatment on selected properties of wheat straws
Document Type
Article
Publication Date
7-1-2009
Abstract
Wheat straw fibers were modified via a pressurized steam treatment. The effect of steam pressure (i.e., 0.2, 0.4, 0.6, 1.0 MPa) and treatment time (i.e., 5 and 10 min) on chemical composition, sorption isotherm, thermal and mechanical properties of the treated fibers was investigated. Differential scanning calorimetry analysis showed that thermal characteristics of the treated straw samples were shifted indicating the improved thermal stability. The ash and extractive content of the treated straw was reduced; and the materials were likely removed when the steam was released. The removal of ash and extractives could improve the wettability of wheat straw when it is used in combination with polymer matrices. Sorption behavior study showed that steam treatment reduced the hydrophilic characteristic of wheat straw. Tensile strength of the treated straw was significantly enhanced. The tensile strength of straw after treatment at a steam pressure of 1.0 MPa for 5 min was more than twice higher than that of the control group. The study demonstrated that pressurized steam treatment is an effective pre-treatment process for wheat straw fibers as possible reinforcement element in polymer matrices. © 2009 Elsevier B.V. All rights reserved.
Publication Source (Journal or Book title)
Industrial Crops and Products
First Page
48
Last Page
53
Recommended Citation
Han, G., Cheng, W., Deng, J., Dai, C., Zhang, S., & Wu, Q. (2009). Effect of pressurized steam treatment on selected properties of wheat straws. Industrial Crops and Products, 30 (1), 48-53. https://doi.org/10.1016/j.indcrop.2009.01.004